What ASTM A268 covers
Standard at a glance
- Standard
- ASTM A268 / ASME SA268
- Issued by
- ASTM
- Product form
- Tubes
- Grades on site
- 4
Covers ferritic and martensitic stainless tubing, including TP409, TP410, TP430 and TP446, for heat exchangers, condensers and general service where chloride stress-corrosion cracking of austenitic grades is a concern.
Key requirements
- Heat treated per grade (annealed)
- Flattening, flaring and hardness tests
- Hydrostatic or non-destructive electric test on each tube
- General requirements per ASTM A1016
Summary for procurement guidance. Refer to the current edition of the standard for full requirements.
Grades supplied to ASTM A268
Ordering to ASTM A268
- State "ASTM A268" and the edition if your project requires it
- Grade / designation and product dimensions
- Supplementary requirements (tests, heat treatment, certification)
- Certificate type: EN 10204 3.1 or 3.2
Frequently asked questions
What does ASTM A268 cover?
Covers ferritic and martensitic stainless tubing, including TP409, TP410, TP430 and TP446, for heat exchangers, condensers and general service where chloride stress-corrosion cracking of austenitic grades is a concern.
Which grades are covered by ASTM A268?
On this site: SS 409, SS 410, SS 430, SS 446.
Do you supply material certified to ASTM A268?
Yes. Material is supplied to ASTM A268 with EN 10204 3.1 certificates (3.2 on request), where the mill certifies to it.
Is ASME SAA268 the same as ASTM A268?
ASME adopts many ASTM material specifications into Section II with an "S" prefix (for example SA-268). The adopted text is identical or includes stated modifications, and dual-certified material meets both.